Any suggestions on a heat treatment cycle for high strenght. The batch anneal shop uses Entec which is ran by a cold spot. The HS cyle is 1175. I beleive the furnance was distrubed. I have four coils of blue steel, and I would like to try to save them and redox them somehow. Any suggestions>>>
 