I had a question about grey water recycling, can grey water recycling systems be applied in building rehabilitation or are they only for new buildings?
On the other hand, can they be used to irrigate all types of plants?
 
Replies continue below

Recommended for you

Hellow mate,

It must have a pH below 3 for use it in concrete

And for irrigation, with normal treatment it can only be used on non-fruit plants.
 
Hello Alvaro, as far as I understand it is possible to use grey water for rehabilitation buildings. To the question of the plants; I agree with Laura and Aitor.
 
Hello guys,
I have already read your answers and these were very helpful.
Thanks a lot!