Mar 25, 2019 #1 ben3929 Civil/Environmental Joined Jan 20, 2010 Messages 35 Location US what type of gasket is recommended to use for water pipe line? water pressure 300 PSI. spiral wound metallic gasket vs EPDM rubber gasket?
what type of gasket is recommended to use for water pipe line? water pressure 300 PSI. spiral wound metallic gasket vs EPDM rubber gasket?
Mar 25, 2019 #2 mk3223 Mechanical Joined Feb 4, 2006 Messages 1,488 Location US Any more detail of the piping info, such as material, operation condition, etc.? IMO, based on the piping material and/or flange joint type, the spiral wound gasket may go with the RF flange, as rubber gasket may be used in the FF flange. Upvote 0 Downvote
Any more detail of the piping info, such as material, operation condition, etc.? IMO, based on the piping material and/or flange joint type, the spiral wound gasket may go with the RF flange, as rubber gasket may be used in the FF flange.
Apr 2, 2019 #3 SnazyDragon Mechanical Joined Aug 13, 2018 Messages 15 Location CA 300# 304 SPIRAL WOUND LOW STRESS FLEX GRAPHITE FILLED CS OUTER RING Commonly used in industry. Check pressure-temperature ratings based on design conditions. Upvote 0 Downvote
300# 304 SPIRAL WOUND LOW STRESS FLEX GRAPHITE FILLED CS OUTER RING Commonly used in industry. Check pressure-temperature ratings based on design conditions.
Apr 8, 2019 #4 KevinNZ Mechanical Joined Jun 12, 2003 Messages 871 Location NZ There are many 'paper' gaskets that suitable for water duty. But if there are water hammer events on your line spiral wound maybe better. Upvote 0 Downvote
There are many 'paper' gaskets that suitable for water duty. But if there are water hammer events on your line spiral wound maybe better.