I'm looking for a rare welding wire. My usual sources have found it but at outrageous prices. Any suggestions?

Metrode 316MnNF or Bohler Thermanit 19/15H. (Equivelants would be fine.)
 
MIG wire would be preferred. Otherwise I'd have to run a hot wire TIG system and I'm not as keen to do that.
 