Hi Everyone,

I have one query regarding radiography marking on ASME U stamped vessels.
As per client requirement Category A (Long seam) & Category B (Cir seam) of shell must be spot radiographed, i.e E =0.85.
But Category A joint of dish with seams must be fully radiographed, i.e E =1.

Kindly advise what will be the marking to be stamped on nameplate.

Regards,
Balaji Rai
 
 http://files.engineering.com/getfile.aspx?folder=dce2176c-2708-48d4-9acb-735ebb52c40a&file=Radiograohy_requirements.png
RT-1 doesn't fit, since the Cat. A of shell is not fully Radiographed.
RT-2 doesn't fit, since the Cat. A of shell is not fully Radiographed.
RT-3 doesn't fit, since Cat. A of head is fully Radiographed.
That leaves you with RT-4.
 
Hi David,

Thanks for your reply.

Regards,
Balaji
 
If you actually have a head seam...

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 