I am looking for an inpsection standard to put on a drawing for radiographic insepction of two welded aluminum parts. Does anyone know where I can get such a standard and an acceptance criteria?
 
Replies continue below

Recommended for you

What code, standard or specification are you working to? If none, what are the parts going to be used for and what kind of parts are they. In additin, what welding process are you using?
 
the aws code for welding aluminum is AWS D1.2 in there is all you need the know about RT criteria.
 