"Superglue" for Concrete Repair

Status
Not open for further replies.

KimWT

Structural
Jul 15, 2003
71

Hi!

I heard precasters use Superglue for crack repair.
I am not sure how this will work in the concrete.
When I search the internet, I cannot find good info related construction use.
I guess this repair method is not popular.

Is this really proper repair product?
I wonder why they do not use Epoxy.

Thanks!
 
Replies continue below

Recommended for you

I can't speak for every precaster but we most certainly do not use Cyanoacrylate for concrete crack repair. We use a proper crack injection repair or surface sealant to repair any cracks deemed objectionable.

Ian Riley, PE, SE
Professional Engineer (ME, NH, VT, CT, MA, FL) Structural Engineer (IL)
American Concrete Industries
 
I have heard Epoxy called the "super glue" for concrete, but don't think it was literal.
 
If it is used for repairing ornamental precast concrete, the only reason I can think of is that it dries clear.

Mike McCann, PE, SE (WA)


 