any tips on how this kind of "knurling" was made on this stainless steel pipe?
1) pipe was not deformed during this proces
2) it is not additionaly welded (however it looks like this) - this surface is "torned out" from pipe material
3) anyone knows machines which can do this type of surface ? (if not - I need to do some R&D'ing on my own)
thanks in advance