I started my work as a Materials Engineer three months ago. Now I have questions on materials selection for drums and heat exchangers in caustic service.
My questions:
1) What is the exact definition of the caustic service.
2) In NACE RP0403-2003 Figure 1, the materials selection and PWHT requirement are determined by the temperature and concetraion of NaOH (wt%). But my supervisor said that the concetraion of caustic included NaOH and other sodium salts (Na2S...). Is he correct?
For example:
The design temperature: 80C
NaOH: 0.5 wt%, other sodium salts: 9.5 wt%
what is the caustic concentraion I should use: 0.5 wt% or 10 wt%.
Please help.
Thanks.
My questions:
1) What is the exact definition of the caustic service.
2) In NACE RP0403-2003 Figure 1, the materials selection and PWHT requirement are determined by the temperature and concetraion of NaOH (wt%). But my supervisor said that the concetraion of caustic included NaOH and other sodium salts (Na2S...). Is he correct?
For example:
The design temperature: 80C
NaOH: 0.5 wt%, other sodium salts: 9.5 wt%
what is the caustic concentraion I should use: 0.5 wt% or 10 wt%.
Please help.
Thanks.