Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Question on A606 steel

Status
Not open for further replies.

ksuengrng

Mechanical
Joined
May 23, 2000
Messages
50
Location
US
Has anyone heard of A606 Type 4 steel. I am working on a project for a client, and they are telling me the tube material is A606 Type 4. I have found nothing in ASME Section II(D), MATWEB.com, or in my Engineering Properties of Steel book.

They also said it is like C1010, and/or A570 Type 50.

Can anyone shed some light on this for me.

Thanks
 
a606 is in astm volume 1.03 high strength low alloy with improved atmospheric corrosion resistance
 
asme may not cover this specification but astm does
 
This standard covers HSLA steels with improved corrosion resistance. The corrosion resistance is provided by the addition of Cu. The nominal chemical composition requirements are as follows:

Cast or heat analysis
C = 0.22 max
Mn = 1.25 max
S = 0.04 max

Microalloy elements are necessary to meet the mechanical property requirements. Examples of these in HSLA steels are V, Nb (or Cb), Ti, etc.

You can obtain more information on this standard using the following link to the ASTM website:

 