hotbat

Mechanical
Sep 13, 2009
5
we have ever used to A193 B7 bolt & A194 2H hex nut in our valve products
but, we have a any problems to purchasing of hex nut such as A194 2H from our vendors
so, we would like to change a material from A194 2H to ISO metric grade nut 12(10.9)

Is it possible?

pls, give a correct interpretation
 
Replies continue below

Recommended for you

This will depend on what standards you want the valve to meet.
 
Thanks you for reply
I will employ to ASME B16.34 and API 6D for Ball valves

pls, give a correct interpretation
 
Status