Qualification of Group II to Group II Materials. AWS D1.1

Status
Not open for further replies.

TimothyM

Materials
Aug 6, 2013
1
Table 4.8 within D1.1 (2010) lists PQR base metal on the left and WPS base metal group combinations allowed by PQR on the right. So with that being said if I qualify a group II material (X52) to a group II material (X52) does that indicate that I am also qualifying group I to group I, group II to group I, and group I to group I?
 
Replies continue below

Recommended for you

Yes, provided all other essential variables are observed.
 