I have an assembly thta I want to coat with QPQ for erosion and galling protection. Nothing to do with corrosion protection. I am worried threads will have a tendency to crack such as during thread make-up at highly stressed last thread.
Should a part that is using QPQ with an API thread have the thread blanked, part QPQ'd and then cut have the API thread machined after which an appropriate coating can be applied? Or is this overkill and do I even need to worry?
Material is Low Alloy Steel , 110ksi 30-36 HRC P110 equiv.