Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

PWHT

Status
Not open for further replies.

blaqesmith

Materials
Jul 13, 2013
45
Dear Experts, Please guide me about following issue
Q # 1
What is minimum thickness for PWHT for storage tank shell, Bottom(Construction code:API 650)?

Q # 2
Where is it written in API 650? please share reference with me?
 
Replies continue below

Recommended for you

Sorry for the double post. If you are asking about shell plate specifically I don't believe the code addresses that.
 
In additional be aware in the materials that quenched and tempered and read ASTM A537-Class 2.

Hope it helps you.
 