Weld overlayed tubesheet need to be PWHT according to ASME VIII div 2.
- Tubesheet : SA336 F22Cl3 thickness 408 mm weld overlay with Inconel 600 thickness 8 mm.
According to the code : P5A group needs 1250°F and for this case 7h 45 min.
Is this correct since AF551 "determing thickness is total thickness of base material".Will we have problems with Inconel ?
- Tubesheet : SA336 F22Cl3 thickness 408 mm weld overlay with Inconel 600 thickness 8 mm.
According to the code : P5A group needs 1250°F and for this case 7h 45 min.
Is this correct since AF551 "determing thickness is total thickness of base material".Will we have problems with Inconel ?