ravivaranasi
Mechanical
- Jul 20, 2016
- 1
Dear Experts,
Could any one please clarify whether PWHT could be waived on the fillet welds for refractory anchors(310 SS mat'l grade) made on a manway cover on the channel side of a waste heat boiler with material grade SA-516-70N built to ASME sec-VIII div-1 but is Non code.PWHT was initially performed because of service.
So do you guys think that the new dissimilar fillet welds with throat thickness being 5 mm can be waived of PWHT requirements even if it is Non code.
if it is non code does exemptions under UCS 56 is applicable...???
Could any one please clarify whether PWHT could be waived on the fillet welds for refractory anchors(310 SS mat'l grade) made on a manway cover on the channel side of a waste heat boiler with material grade SA-516-70N built to ASME sec-VIII div-1 but is Non code.PWHT was initially performed because of service.
So do you guys think that the new dissimilar fillet welds with throat thickness being 5 mm can be waived of PWHT requirements even if it is Non code.
if it is non code does exemptions under UCS 56 is applicable...???