If the heat exchange tube side in sour water service (or caustic, amine service, is PWHT required for tube to tube sheet welds?

Thanks.
 
Replies continue below

Recommended for you

No, you cannot PWHT the tubesheet + tubes because there is risk of breaking the weld (by the way, breaking the strength of tube expansion also), due to differential expansion of the assembly in the furnace.
Cheers,
gr2vessels
 
I heard that the manufacturer perform PWHT for Cr-Mo tube to tube sheet welds. Is it true?
 