Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

PWHT of ASTM-A336-F11-3 Heat Exchanger in accordance with PD5500

Status
Not open for further replies.

CuMo

Mechanical
Joined
May 1, 2007
Messages
152
Location
GB
Hi all.
We are designing a BEU heat exchanger to PD5500
where shellside cylinder, tubesheet and shellside dished end are forged from ASTM-336-F11-3 (UNS K11572).

Tubeside channel is a known territory so nothing to worry about here.

Due to thickness shellside components are subject to PWHT.

ASTM A336-F11-3 isn't listed in PD5500. There are some CrMo listed in Table 4.4-1
but classification is to BS EN 10222-2 (For forgings).
My first reaction was to compare chemical compositions but nothing really matches 100% so I gave up.

Then I had a look in ASME IX and ASME VIII-1
where for P4 materials a minimum holding temperature of 650 deg C is recommended.

Some refinery specs which I have access to describe P4 materials as (1.25 Cr – 0.5 Moly) and suggest
a PWHT temperature range of 1275 deg F +/- 25 deg F ( 677 deg C to 704 deg C)

I believe I'm on the right track but can't find a route or statement in PD5500
which I can use to justify my approach.

Any comments welcome!
 