Yasir Irshad
Mechanical
A Section VIII, Div. 1 vessel was originally PWHT for code related reasons only. However, the vessel is not stamped. An R Certificate Holder while modifying the internals, welds a 10 mm thick demister support ring internally with the shell of 50 mm thickness by fillet welding. The weld throat thickness is 7 mm. The material of construction is SA516-70. Does this fillet welding of 10 mm thick support ring has to undergo PWHT? If yes, then which clause of Sec VIII or NBIC mandates it?
Note: Service of this vessel doesn't require PWHT.
Please clarify