UW-40(a)(4) permits "heating the vessel internally by any appropriate means ...".
Sect. I PW-39.4 does not specify internal or external heating.
There are companies who perform PWHT by shooting a flame into the interior of a vessel in order to obtain the required temperature. I have also heard of chemical exothermic reactions from the inside as well.
Some large consultants do not accept any method other than heating the entire vessel in a furnace but I suspect that alternatives are used successfully.
Does anyone have experience with these alternate methods?
Are there other methods that are used?
Any problems with such alternate methods?
Thank you.
Sect. I PW-39.4 does not specify internal or external heating.
There are companies who perform PWHT by shooting a flame into the interior of a vessel in order to obtain the required temperature. I have also heard of chemical exothermic reactions from the inside as well.
Some large consultants do not accept any method other than heating the entire vessel in a furnace but I suspect that alternatives are used successfully.
Does anyone have experience with these alternate methods?
Are there other methods that are used?
Any problems with such alternate methods?
Thank you.