Dears frds,

pls clarify, How to find heat treatment of pwht holding temperature and holding time?
in material sa-516 gr 70(NACE+ HIC)


thanks & best regards,
saravana
 
Rd th Cde :)

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 
HIC + NACE material would require some extra holding temp and time apart from the minimum requirements of the ASME BPVC code. Usually these requirements are given in a client material Specification. Please demand these specs from your client / process licencor/ EPC Contractor.

 
See:
NACE SP0472
NACE 8X194

Regards

 
Or, retain a professional welding engineer