Doing a SS overlay onto carbon steel. Does anyone know where I can find PWHT requirements? Doing to ASME 8 and 9. Any guidance would help.
 
Replies continue below

Recommended for you

If this is for a pressure vessel, the PWHT exemptions for a corrosion resistant weld overlay applied on a carbon steel substrate can be found in ASME B&PV Code, Section VIII, Div 1, Part UCS. See Table UCS-56.
 