Is PVDF (Polyvinylidene Fluoride) chemically compatible with DNT (Dinitrotoluene) and MNT (Mononitrotoluene) at 70 C?
 
Not listed. Nitrobenzene (very similar chemical) is listed at room temperature only and is rated 7-8. Based on the ratings I'm seeing for other related plastics at elevated temperature with nitrobenzene I'd be hesitant to use it with PVDF. Ask the manufacturers.

Chris DeArmitt PhD FRSC
President

Plastic materials consultant to the Fortune 100
Creating New Materials - Problem Solving - Innovation Keynotes - Expert Witness
 
Several articles cite that liquid dinitro toluene attacks some form of plastics, rubbers, and coatings with no further details. Is it possible a common molecular structure/Bond that DNT reacts with, such as C-H bond?

After looking into several chemical compatibility charts, it appears that only few materials can handle DNT, including PTFE and FFKM and some other metallic material.
 