Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

pvc versus chlorinated pvc

Status
Not open for further replies.

corrosionman

Mechanical
Jun 11, 2003
214
In an emergency situation we had to modify some 2" cpvc pipework but using pvc instead (due to material availability.) The duty is ambient temp Chlorine Dioxide at 5 bar pressure. As best we can deduce from corrosion charts pvc is inferior to cpvc, but maily at elevated temps. At ambient, there does not seem to be much difference. We plan to replace the incorrect pipes but are trying to decide if really necessary. Please has anyone any comments.
Thanks.
Corrosionman.
 
Replies continue below

Recommended for you

I seem to remember that PVC doesn't do as well as CPVC in two other situations...

1) sunlight (UV)
2) flex

So beware if you're stringing this stuff out in the sun in a pipe rack intended for large bore steel piping.