I have a great video of a PVC pipe fitting being tested to failure. Video is best I have ever seen demonstrating the cyclic failure PVC pipe fittings.

I would like to use this video but I have no reference to where it came from or who made the video. I would like to have their permission to use it.

I think this video came from an engineering firm that did a study for IBM to find out why their PVC fittings were failing so often. Video may have come from a plastics conference many years ago.

Anyone know? Please send any references you have.


I have posted the 10 MB video temporarily at this link: