Can someone please explain what does PV1200 exposure actually is, as well as TL211?


Thank you very much,

Regards,

Andrei M.​
 
TL 211 is a standard from Volkswagen, with the title Paint Coating on Exterior Plastic Parts.

PV 1200 is another standard from Volkswagen, with the title Aggregate, Bauelemente, Systeme, Halbzeuge - Klimawechseltest.

You can contact VW for more information.
 