Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations LittleInch on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Puzzling Question for Stress Relief Gurus

Status
Not open for further replies.

jackboot

Mechanical
Joined
Jun 27, 2001
Messages
151
Location
US
I have a theoretical question.

Question: I have a hollow thin-walled cylinder. I put it in a press and plasticity deform it in the lateral direction. At this point, I have an oval shaped "cylinder." If I stress relieve this part - will the cylinder move towards its initial round shape?

Or what direction would it move, or does it move at all?

jackboot
 
If you have plastically deformed the metal there will be no appreciable change in shape if the stress relief temperature is below 1150°F
 
To add to unclesyd's comment, the key is if you have permanent deformation -which you indicated. The permanently deformed material will not appreciably move without any additional force applied at or above 1150 deg F. This additional force at temperature is required to permantly deform the material back in the opposite direction - similar to re-rounding a cylinder.
 
The 1150 F temperature applies to steel, and not to non-ferrous metals like aluminum and magnesium.
 