Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations KootK on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

pump for molten zink

Status
Not open for further replies.

srgnt

Mechanical
Apr 11, 2001
3
I need a positive displacemant pump to pump molten zink at five gpm and 100 psi. Does anyone know where I can get one?
 
Replies continue below

Recommended for you

With regard to your need for a "molten Zinc pump"

I suggest that you contact the technical rep's at Viking Pump...


They have experience with this type of "hot metal" pump and have supplied pumps for both lead and zinc.

The pump is an internal gear, positive displacement pump without a seal ( Your pump efficiencies are going to be low)

The real trick..... in the plant layout, is to keep the motor cool

Good Luck


MJC
 