Hello All,

We have performed the Pull off adhesion test for vessel plate ( mat'l 516-60N +HIC), test type is
self aligned adhesion tester in ASTM D4541, the accepable range is more than 10 Mpa. but in three sample
two were failed.

Now my query is there any co relation on DFT to faliure of adhesion test, as we need to apply 500 micro
and i saw our sub contractor applied more than 750 micro. so is it that more the DFT more tha possibility of faliure
of adhesion test ?

Please advise as i am quite new on this feild.
 
Thinner coatings give better adhesion. Better to apply two thin coatings than one thick.

Chris DeArmitt - PhD FRSC CChem
Plastic & Additives Webinars
Instant Downloads & Inexpensive
 
While it is generally true that thinner coatings yield better adhesion, most adhesion failures are due to poor substrate surface conditions, meaning excessive contamination, poor cleaning, etc.
 
What kind of paint you are working with ?
As already said, is it a one coat system or multilayer ?
We also need to know where the break occurs to have an idea of the why this happen.
- Inside the paint
- Interface glue/paint
- Interface paint/substrate
- if multilayer, interface layer/layer