Or in short, use of trade names may help.
PTFE = Teflon
PCTFE = Kel-F
Both are suitable for use for ball valve seats. Big difference is the PCTFE is harder and has higher friction. Impact of both factors is that it tends to require more torque to turn the valve open and closed.