Jul 16, 2016 #1 ryz049 Aerospace Joined Jul 16, 2016 Messages 1 Location IN how to run strain controlled fatigue test, knowing pseudostress range & R ration?
Jul 19, 2016 #2 mp87 Materials Joined Jan 27, 2015 Messages 55 Location FR Given the few information provided, here is the best source I can address you to: ASTM E606 / E606M - 12 Standard Test Method for Strain-Controlled Fatigue Testing Upvote 0 Downvote