Dear sir

I have faced a situation where pipe has corroded internally. Suggest protective lining inside pipe its is dia 16". Length around 200ft.
Length of pipe welded together

Regards
 
The first question is does the corrosion threaten the integrity of the pipe?
If the pipe is still mechanically sound then you can look at ways to clean the inside and have a plastic lining installed.
But maybe you also try to figure out how to stop the corrosive material from getting into the line.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy
 
One concern is that the process may be contaminated as the internal coating was chipped out for some reason.
You may suggest to investigate what is the corrosion mechanism of the pipe, and consider to upgrade the pipe material to eliminate the corrosion issue.
 
Dear Sujoo94,

You can eliminate the problem if you install driers. But that could be expensive.

Regards.

DHURJATI SEN
Kolkata, India

 
If it's anything like the service air systems in my fleet all of the piping is below the receivers so the receivers will be in great shape.
 