hi

can any one give me the material information for forged steel 1035.

mainly, i want to know the yeild strength of this FS 1035.
i am doing analysis on Forged Steel Clevise.

please help me out.
 
Can you be more specific about the specification and any heat treatment th ematerial received?
 
I am doing a structural analysis on this Forged Steel Clevise.

It is aupplied by MCMaster CARR. They didnt even specifiy the material in particular. U could find the part easily when u search in the catalog in McMaster wbsite for " Forged Steel Clevises"

I called them and asked for details and all they told is that they use FS 1035.

But to compare my stress results i have to atleast know the yeild stress.

I will be very happy if u can help me out.
thanks

Sarita
 
You can get into big trouble trying to do engineering with catalog parts. Even if you bought one and had the hardness checked (which would get you "ballpark" yield strength with some conversions and interpolation), you have no guarantee that the material and yield strength would not change at some future date, rendering your analysis worthless.
 
Without knowing the specified heat treatment as mentioned by carburize, an alternative approach in this structural analysis could be to use normalized mechanical properties for AISI Type 1035. If the clevice was required to be heat treated after forging to provide a minimum yield strength value, using the yield strength for a normalized condition would allow you to evaluate how much safety margin is in the design of the clevice. Heat treatment would serve to increase the yield strength and increase design margin in comparison to mechanical properties in the normalized condition.

0.2% YS for AISI Type 1035 hot rolled and air cooled is reported to be ~40 Ksi (source;
 
Thanks both of u for ur suggestion. i hope my boss agrees with this.

Sarita
 