Properties for a W21x49 and a W21x55

Status
Not open for further replies.

ars13

Structural
Feb 11, 2009
33
Does anyone have the structural properties for a W21x49 and a W21x55 or where they could be found? Thanks
 
Replies continue below

Recommended for you

W21x55 is a standard shape in the AISC manual. Not familiar with the W21x49 shape. There is a W21x48 and a W21x50 available, however.
 
From the AISC 7th Edition
W21x55
A=14.4
d=20.82
Ix=971
rx=8.21
Iy=24.7
ry=1.31

W21x49
A=16.2
d=20.8
Ix=1140
rx=8.40
Iy=48.3
ry=1.73
 