Jun 2, 2002 #1 menbom Mechanical Joined Jun 2, 2002 Messages 2 Location AU I am investigating a fractured cam shaft which I believe is made from a proferal cast billet. I think this is a grey cast iron, but do not know to what specification. Can anyone assist?
I am investigating a fractured cam shaft which I believe is made from a proferal cast billet. I think this is a grey cast iron, but do not know to what specification. Can anyone assist?