Hello

Can anybody shed some light as to how free-standing, sub-micron foils are made? I know most metals can be reduced to a submicron thickness via a combination of rolling followed by beating as is done with the production of gold leaf - however foils made in this fashion are riddled with numerous pinholes and consequently lack density. Somebody in a post mentioned an optimal alternative is “evaporation”. But aren’t evaporation techniques employed exclusively for permanent thin film deposition on to a substrate? How I wish he had elaborated. Anyway, hope somebody out there can help me understand.

best
vas
 
Replies continue below

Recommended for you

Thank you all for the recommendations, we will definitely look at the proposals at our leisure.
 
Wow! Thank you IRstuff. This place is a wealth of information!! If you got anything else please share.
 