Hi,

I have experimental data of a compressed test with Stress-Strain graph like shown below.
In linear elastic region, Stress/Strain do not equal Young modulus.
How can I use this data and reproduce the experiment in ansys./

Thank you,
 
 https://files.engineering.com/getfile.aspx?folder=bd11fe0b-f053-4d49-b8a0-d1cf59d6eb7c&file=compression.PNG
But Young modulus is determined by Stress/Strain in linear elastic region.
 
Yes, but in that grap, linear elastic region, relationship between Stress-Strain is not Linear, which is the curve. I dont understand it
linear_nygpjr.png
 
It says 'cell walls bend', are you working on some sort of honeycomb structure?
 