Hi,

I'm tring to model a forging process with ABAQUS/Explicit, but I've got a problem with self contact (or maybe surface définition). one surface of the elastic-plastic material is schrivelling up during the simulation and after a certain elapsed time one of my boundary node is moving inside the matérial, making the simulation failing.

I defined my surface like this (I aslo tried without the internal surface, without succes, and my elements are CAX4R):
*Elset, elset=S1, instance=lopin, generate
1, 150, 1
*Elset, elset=S1_int, internal, instance=lopin, generate
1, 150, 1
*Surface, type=ELEMENT, name=S1
S1_int, S1

The contact is defined with:
*Surface Interaction, name=contact
*Friction
0.2
*contact Pair, interaction=contact
S1, S1

Any advice would be very appreciated, thanks in advance!

François.
 
Hi again,

While I was trying to solve my problem I ran the example problem "ale_sinusoid_forgingaxi" (contained in Abaqus example problem manual, section 1.3.9) to see how it was defined. Exactly the same problem happens at the end of the simulation if I divide de velocity by 10 and multiply the simulation time by 10.

Could someone explain me why some nodes/elements don't react correctly in this case?

I've made a lot of attempts to solve this, without succes, and my work is blocked...Thanks in advance!

François.
 
Hi Francoisgl

Regarding your contact problem, you could look at using general contact rather than the contact pair algorithm. Look at *CONTACT and *CONTACT INCLUSIONS.

Good luck!

Martin
 
Agh, my mistake - just re-read the original post and I see that you are using axisymmetric elements. I believe that the general contact method is only available for 3D elements, so it won't help you at all I'm afraid.

Martin
 
Ok, no problem, Martin...

Still trying to understand why the "ale_sinusoid_forgingaxi" failed, I just tried to divide the analyse in two steps (I was only using one step), specifying the option op=new for adaptive mesh, and I got a solution!

So maybe it will work for my work... I'll give news soon, it would maybe be helpfull for others.

Thanks anyway, Martin,

Francois.
 