Hello,
New to this forum. We have Amada 4020NT and regularly cut 1/2" material with this machine. I'm having trouble with a sheet 72"x144". Clean sides but thin dross bead on bottom. I think my problem is bottom surface quality but I was hoping for suggestions.
Current settings: 7" lens, 1.4D nozzle, 0.022 focus, 31 ipm, 2500 Watts, 1200 freq, 80 duty, 0.06 gas pressure, .055 gap.
I've tried 45 ipm, 4000 W, 2000 freq, 100 duty, .08 Mpa. but I get magma on top side like it cant push through.
Any help appreciated
Jef
New to this forum. We have Amada 4020NT and regularly cut 1/2" material with this machine. I'm having trouble with a sheet 72"x144". Clean sides but thin dross bead on bottom. I think my problem is bottom surface quality but I was hoping for suggestions.
Current settings: 7" lens, 1.4D nozzle, 0.022 focus, 31 ipm, 2500 Watts, 1200 freq, 80 duty, 0.06 gas pressure, .055 gap.
I've tried 45 ipm, 4000 W, 2000 freq, 100 duty, .08 Mpa. but I get magma on top side like it cant push through.
Any help appreciated