Dear All:
In my plant we have a recovery boiler system that burns Production byproducts to produce steam. This system has been working for around 15 months and we are experiencing a problem that I would like to share with you:
The system is composed by a combustion chamber where the byproducts (sometimes extremely acidic with a HCl content of 10%) are burned at a temperature of 1100C, and then these gases go to a double pass boiler to produce steam. The exit temperature of those gases to the gas treatment part of the system is around 400C.
My problem is that the tubes of the boiler are breaking. This failure always happens in the first pass of the boiler and there are already 3 broken pipes (that were closed with a metal disc). The first pipe broke in Feb last year, so 5 months after the start up, then the other two pipes broke around one month ago.
The system is stopped and cooled down to almost ambient temperature in average 1 time/week to clean the boiler due to salt formation in the tubes
Any clue of what is provoking these failures?
Thanks a lot for your help
In my plant we have a recovery boiler system that burns Production byproducts to produce steam. This system has been working for around 15 months and we are experiencing a problem that I would like to share with you:
The system is composed by a combustion chamber where the byproducts (sometimes extremely acidic with a HCl content of 10%) are burned at a temperature of 1100C, and then these gases go to a double pass boiler to produce steam. The exit temperature of those gases to the gas treatment part of the system is around 400C.
My problem is that the tubes of the boiler are breaking. This failure always happens in the first pass of the boiler and there are already 3 broken pipes (that were closed with a metal disc). The first pipe broke in Feb last year, so 5 months after the start up, then the other two pipes broke around one month ago.
The system is stopped and cooled down to almost ambient temperature in average 1 time/week to clean the boiler due to salt formation in the tubes
Any clue of what is provoking these failures?
Thanks a lot for your help