Hi,

We have bucket type mesh filters installed at our plant after the furnace where we have VCM in addition to craked EDC , HCL and some amount of coke. Filters are of SS 304 and mesh size is 20, installed at pump suction. However, whenever we open them, mesh found dislodged from its body and damaged from various places in addition of coke in filters. Can anybody will help me out in this issue
 
Replies continue below

Recommended for you

Stress corrosion cracking due to presence of chloride ion and high temperatures?

Good luck,
Latexman
 
Ok, dear But whats the long term solution of this problem
 