Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Price Levels 1

Status
Not open for further replies.

dragos12

Civil/Environmental
Joined
Sep 18, 2005
Messages
27
Location
TR
Can someone a price comparison for materials like below?
WCB, CF8M, Alloy 20, 904L, Inconel 625, Hastelloy C276, etc.
Like 1: 2 : 2.5 : 2.5 : 6 : 7 etc
 
as what, plate?
In general 625 and C276 have very similar prices, about 8-9x the 304 price.
Alloy 20 and 904L are used very little, so they are more expensive than the alloy content would indicate.
At todays Ni and Mo prices 316 is about 1.4x the 304 price (hence the move to lean duplex grades in place of 316).


= = = = = = = = = = = = = = = = = = = =