Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations 3DDave on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Pressurized DA tank inspection

Status
Not open for further replies.

Jazzerman

Mechanical
Nov 17, 2013
12
Can anyone help me with requirements vs recommendations on DA tank inspection? Hospital client with central steam plant, with pressurized DA tank operating at 5 psi. I assume relief valves set at 15 psi but have not checked. I would figure an annual inspection inside the tank is smart, but is it required by code (ASME or other)?
 
Replies continue below

Recommended for you

For a DA tank, it would be wise to perform an internal inspection. In states or cities which regulate pressure vessels, these could be considered as corrosive service which would require access to the internal surface as part of a 3 year Jurisdictional inspection. Each State or city has their own rules for what is required for inspection to obtain an Operating certificate.
 
Some relevant DA inspection/failure information here:





It is important to recognize a few features about deaerators:

1) They are usually (fairly) large vessels designed for low pressures and therefore somewhat fragile. As they age, there is little or no margin in the design. For any vessel designed to a design pressure of less than 15 psig, the ASME rules on quality, testing and inspection DO NOT apply. There have been catastrophic DA failures in the past that have killed people.

2) In the 1990s, the heat exchange institute and NACE recognized this significant hazard and issued recommended guidelines for design,inspection and construction.

3) Deaerators are somewhat unique as they are commonly subject to internal impact forces during normal operation and therefore experience an accelerated degree of cracking and failure. Many, many internal trays have become loose and caused internal damage...

My opinions only

-MJC




MJCronin