I have to use a pressure transmitter with a flanged (Raised Face rating 600#) diaphragm seal on a the on the outlet of a well. The material engineer specified that the wetted parts shall be Hastelloy-C, so i chose the diaphragm material to be hastelloy-C. What should the diaphragm seal flange material be? should it be Hastelloy-C as well ? or is it ok to use a carbon steel flange, and rely on the gaskets to make the process fluid does not contact the flange ?
Also note that i can not use 316 SS flange because this will lead me to increasing the rating to 900# instead of 600#, as piping is working at the edge of rating 600# for carbon steel.
With regards to carbon steel, i am worrying about galvanic corrosion between the seal carbon steel flange and the hastelloy-C flush ring.
What do you think ?
Also note that i can not use 316 SS flange because this will lead me to increasing the rating to 900# instead of 600#, as piping is working at the edge of rating 600# for carbon steel.
With regards to carbon steel, i am worrying about galvanic corrosion between the seal carbon steel flange and the hastelloy-C flush ring.
What do you think ?