pressure transmitter housing

Status
Not open for further replies.

hsme

Mechanical
Nov 2, 2013
2
Hello all
for housing of pressure transmitter on offshore platform what provisions shall be considered if we want to use aluminum housing, like coating, copper content, etc,...
with the provisions considered for aluminum how different it is with stainless steel housing.
thank you
 
Replies continue below

Recommended for you

You should refer to NORSOK Standard M-001 Materials selection.
 