I need to determine the ratings for PN64 flanges in 316L stainless.

So far I've found a german copy of DIN2636 consisting of just a drawing and a page of dimensions, am I missing something?

My copies of BS4504 and ISO7005 don't include PN64.

Any suggestions where else to look?
 
Hi Andrew,
You may refer to the following standard for the pressure temperature ratings of PN64 flange in SS316L material.
prEN 1092-1.

Regards,

Pras
 
Checkout also thread thread292-17262

Especially Fawkes answer from april 10 gives some useful info about the difference between ISO 7005 and EN1092 - also with respect to pressure ratings.