Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Pressure-Temperature Rating for MSS SP-114 150 Class Fittings

Status
Not open for further replies.

AtticusMech

Mechanical
Aug 24, 2017
4
Hello, I'm looking if somebody can advise me what the pressure-temperature ratings of MSS SP-114 Class 150 SS fittings are? I've heard that the equivalent P-T rating of threaded Sch 40 pipe should be used. Can anybody confirm if this is correct? I don't have access to the code and don't want to purchasing it to lookup this one item.

Thank-you
 
Replies continue below

Recommended for you

As per MSS SP-114 2007;

2. PRESSURE-TEMPERATURE RATINGS
2.1 Pressure-temperature ratings for these fittings
are shown in Table 1. Ratings are independent...

[Please website for full standard]
 