I have a need to measure pressure and flow of steam at 450 psi and 1200 degrees F. I am having trouble figuring out how to connect the instruments to the process since 1200 F is above the recommended limit for 316 ss tubng. I can't find gauge siphons or pigtails rated above about 800 deg F. Any suggestions would be appreciated.

Thanks

TWCE
 
Twce - Looking at the ASME tables 316L is limited to 850°F. Using 316, 304, 321 and 310 St. St. is allowed up to 1,500 °F
If using 1500# rating material 316 St. St. allowed for 450 psi at 1350°F.
 