Is preheating necessary when using a gun to weld shear studs? AWS D1.5 (2005) doesn’t require preheating. However we have a project that requires preheating in accordance with Table 4.4.
The contractor doesn’t want to preheat because it’s damaging the paint system and causing some localized buckling of the stay-in-place forms. The stud manufacturer says preheating is unnecessary and the DOT never enforces this provision.
Years ago when I worked as a construction inspector no one used preheating for studs and we never had a major problems. There was the occasional partial flash but that was it.
Any thoughts?
The contractor doesn’t want to preheat because it’s damaging the paint system and causing some localized buckling of the stay-in-place forms. The stud manufacturer says preheating is unnecessary and the DOT never enforces this provision.
Years ago when I worked as a construction inspector no one used preheating for studs and we never had a major problems. There was the occasional partial flash but that was it.
Any thoughts?