albaweld

Petroleum
Jul 23, 2007
29
I'm trying to create a PQR for low temp carbon that will give me both impact values and also PWHT values. I also need this procedure to be utilized when parent metal thickness does not require PWHT. Can I achieve all this on one PQR?
 
Replies continue below

Recommended for you

Essentially 2 PQRs will be required. One qualified with PWHT and one without PWHT.

 